Each case is one decision,
not a success story.
Customer names and part numbers are withheld. The numbers under each case are the process limits published on our own capability pages - they describe what the route is capable of, not a measured result from one customer's program.
The seal face is formed.
Only the seat is turned.
The part. A copper post for a prismatic or blade cell. It carries the current, holds a hermetic seal against the electrolyte, and gives the busbar a flat face to weld to - three jobs in a part that looks like it was simply turned.
The constraint. Copper is the most expensive thing in the part, and a chip is copper you paid for and then sold as scrap. Cutting the whole body from bar also slices the grain across the sealing seat, which is exactly where a leak starts.
The route. Cold heading forms the body and the sealing face in one six-station cycle, with scrap limited to the cut-off. Only the features that genuinely need a cut - step, thread, weld face - go to the lathe, in the same plant, off the same datum. Plating follows without the parts leaving the building.
What it changes for you. One supplier for three operations, one inspection report covering all of them, and a sealing face whose grain runs around the seat instead of being cut through it.
| Material | Copper C1100 / C1020; nickel on request |
| Formed | Cold heading, six stations |
| Machined | CNC turning, Rz 0.8–1.6 µm |
| Supplied | Formed blank, or finished and plated part |
| Documents | PPAP Level 3 · traceable by heat number |
A thin wall is formed,
not bored out of solid.
The part. An air spring piston: a cup with a closed end, a sealing surface on the outside and a bore for the strut, in a wall that gets thinner with every model year.
The constraint. Deep-drilling a thin wall is the most expensive shape there is. More than half the billet leaves as chips, and at the last pass the wall springs away from the tool. Wall thickness stops being a material question and becomes a machine's limit.
The route. Cold extrusion pushes the cup in one stroke - deep blind bore, closed end, uniform wall - at above 80% material utilization. Turned surfaces come off the die at Ra 0.2–0.6 µm, so the sealing seat needs far less cutting, and a warm-forming variant covers the micro-alloy grades that would otherwise need an interstage anneal.
What it changes for you. The wall is set by the punch and the die in the same part. Six hours of drilling at the lathe, plus half the steel you paid for stays in the part.
| Material | 20#, 45#, 40Cr; warm-forming variant for micro-alloy |
| Formed | Cold extrusion - deep blind bore, thin wall cup |
| Machined | CNC turning for the sealing seat and bore |
| Finish | Zinc or manganese phosphate |
| Documents | PPAP Level 3 · FMEA · control plan |
One pitch error, not a stack of them.
The part. A clutch disc hub: an internal spline that has to slide on the input shaft without backlash, riveted to the disc, and hard where it wears.
The constraint. Spline pitch error is what a driver hears as rattle and what a transmission testbed measures as backlash. Split across separate operations, the error of each one stacks; done hot, the spline moves again in the quench.
The route. The blank is cold-headed, then the spline is broached in a single stroke with roughing, semi-finishing and finishing on the same tool path - pitch error held to ≤0.015 mm on series, blind splines included using step-wheel tooling. Hardening is induction and localised: the zone that wears reaches 58–65 HRC while the spline that locates does not move.
What it changes for you. No fit-up operations between heat treatment, and the hardness report and the dimensional report describe the same part.
| Material | 40Cr, 45# |
| Route | Cold heading → broaching → induction hardening → temper |
| Profiles | Involute, parallel-key, serration, custom internal forms |
| Documents | PPAP Level 3 · hardness and case depth per lot |
A contact edge is sheared
bright, not milled.
The part. A knife contact or fuse tag: flat, thin, with a sheared edge that has to be square over its full thickness, because that edge is what carries the current into the clip.
The constraint. A punched edge has a shear band, a break zone and a roll-over. On a contact the break zone is where resistance rises and where plating baths into a crack. Milling the edge square works - and adds a second operation on every piece.
The route. Fine blanking shears the full thickness bright, with die clearance held at 0.5–1% of thickness by wire EDM so the edge is square as sheared, holes go down to 50% of material thickness, and strip up to 10 mm runs in one hit. Silver or nickel plating then goes onto an edge with no break zone to plate into.
What it changes for you. The secondary milling operation disappears from the route, and the edge the current crosses is the edge you specified on the drawing.
| Material | Copper, brass, silver-plated steel |
| Route | Fine blanking or progressive die → finishing → plating |
| Holes | Down to 50% of material thickness |
| Documents | PPAP Level 3 · plating thickness on first-off |
Three things every one
of them depended on.
Take any of the fifteen part families and the questions are the same four: what is formed, what is cut, where the tolerance lives, and who signs the report.
One route, one report
Eighteen processes in 20,000 m², nothing subcontracted. The datum that is formed is the datum that is measured, and one inspection report covers the whole part.
The die is ours
Six die families designed, cut, heat treated and coated in house. An engineering change is a die change in the next bay, not a new supplier qualification.
Documents from the enquiry
PPAP Level 3, the process FMEA and the control plan are written into the route before the first chip, so the paperwork ships with the first lot instead of weeks behind it.
Send the part. We will
tell you which of the four
decisions it turns on.
A drawing with material, annual volume and the tolerance on the functional features is enough to name the route, the operations behind it, and where the cost actually sits.